Follow step-by-step instructions on how to weld a horseshoe pumpkin using the Handler® 210MVP™ MIG welder. 

Tools and Materials Needed:

Steps:

Horseshoe Pumpkin step 1
Buy 9 horseshoes of the same size, cut one horseshoe in half.
Step 2 Horseshoe Pumpkin
Lay 2 horseshoes facing each other and leave a 3/16" gap.
Step 3 Horseshoe Pumpkin
Tack weld together.
Step 4 Horseshoe Pumpkin
Position the next horseshoe at a 90-degee angle and then weld together, repeat 1 time.
Step 5 Horseshoe Pumpkin
Position the next horseshoes at a 45-degree angle and then weld together, repeat 4 times.
Step 6 Horseshoe Pumpkin
Tack and weld the half horseshoe to the pumpkin to create a stem.