How to MIG Weld a Fire Pit

Tools and Materials Needed


Optional:

  • Scrap Metal
  • Grinder
  • Clamps
  • Paint

Material Dimensions


Top Frame: 4 - 1.5" x 1.5" x .125" angle iron x 36" L (cut ends at 45 degrees)

How to MIG Weld a Fire Pit Material Dimensions

Legs: 4 - 1.5" x 1.5" x .125" angle iron x 18" L

Side Vertical Supports: 4 - 1" x 1" x .060" tubing x 33.5" L

Side Bottom Supports: 9 - 1" x 2" x .060" tubing x 8.5" L

Bottom Leg Supports: 4 - 3" x 3" x 3/16" flat stock (optional if fire pit on soft surface)

Pit Sides: See drawing

 

Fire Pit Project Plans