Follow step-by-step instructions on how to create a horseshoe sunflower yard art using the Multi-Handler™ 200 Multiprocess Welder.

Tools and Materials Needed


  • Hobart® Multi-Handler™ 200 Multiprocess Welder
  • Rebar: 1/2” D x 20-3/4” L
  • 7- Horseshoes: size 1

Horseshoe Sunflower Yard Art Project Plans

Download
  • Multi-Handler 200 Package 500578

    Multi-Handler 200

    120/240V. MIG, flux-core, Stick, DC TIG; welds up to 3/8 in. steel 5/3/1.

  • Inventor Series Realtree CamoEdge RF 770875 PC

    Inventor™, Realtree® Camo-Edge

    High-performance auto-darkening helmet. 9.3 sq. in. PureColor lens, grind mode, 4 arc sensors.

  • 770568 Cotton Welding jacket XL

    FR Cotton Welding Jacket, XXL

    Lightweight XXL FR cotton welding jacket. Long sleeves, heavy duty snaps, warm coverage.

  • Step 10 Butterfly Plant Holder Project
    Project

    How to MIG Weld a Butterfly Plant Holder

  • Chimenea Project Plan
    Project

    How to MIG Weld a Chimenea Fire Pit

  • Farm Gate
    Project

    How to MIG Weld a Farm Gate

  • Feed Panel
    Project

    How to MIG Weld a Feed Panel

  • How to MIG Weld a Fire Pit
    Project

    How to MIG Weld a Fire Pit

  • Project Plan Hanging Chair
    Project

    How to MIG Weld a Hanging Chair

  • Welcome Sign Project Guide
    Project

    How to MIG Weld a Welcome Sign

  • Final Sunflower Yard Art Project
    Project

    How to MIG Weld Horseshoe Sunflower Yard Art

  • Lighted Globes
    Project

    How to MIG Weld Lighted Globes

  • Final Yard Cup Holders Project Edit
    Project

    How to MIG Weld Yard Cup Holders

Connect With Us

Subscribe to Hobart News

Sign Up
Cookie Policy
Privacy Policy
Terms of Sale
Terms of Use

© Hobart Welding Products