The Champion® line of engine driven welders provides DC stick welding on steel, stainless steel and cast iron. Use the auxiliary power for tools to get the welding job done quickly and efficiently.
145A engine-driven stick welder. Welds up to 1/4 in. steel. 4,500W surge, 4,000W continuous power