Flux Coated Bronze Gas Welding Rod 3/32 in. x 18 in., 8 pk
770512
Selection Option
About The Flux Coated Bronze Gas Welding Rod 3/32 in. x 18 in., 8 pk
Low-fuming bronze gas welding rods. Copper-tin alloy flows easily to join cast and malleable iron, galvanized steel, bronze, copper and steel. Melts at 1630°F, yields joints up to 63,000 PSI.