7014 3/32 in. Stick Electrode, 1 lb.
H114232-R01
Selection Option
About The 7014 3/32 in. Stick Electrode, 1 lb.
Ideal for high-deposition jobs requiring light penetration and faster travel speeds. 70,000 PSI tensile strength. Runs in all positions on AC or DCEN (straight) and DCEP (reverse) polarity.
Tech Specifications
Discover technical info about this product
Owner's Manuals
Find replacement parts and get the most from your products by downloading the specific Owner's Manual for your unit.