6011 1/8 in Stick Electrode, 1 lb.
H112244-R01
Selection Option
About The 6011 1/8 in Stick Electrode, 1 lb.
Hobart all-purpose stick electrode for all positions on carbon and galvanized steel. 60,000 PSI tensile strength. Deep penetrating for light to medium dirty, rusty or painted materials. Runs on AC or DCEP.