ER308L Stainless Wire .030, 2 lb. Spool
H522506-R19
Selection Option
About The ER308L Stainless Wire .030, 2 lb. Spool
An extra low carbon wire for the welding of type 304L, 321 and 347 stainless steels. Provides excellent notch toughness at very low temperature, and deposit a maximum of .04% carbon in the weld metal to minimize the formation of chromium carbides and consequent susceptibility to intergranular corrosion.