Copper-coated Steel (RG-45) Oxy-acetylene Gas Welding Rod, 3/32 in. x 18 in., 8 pk
770514
Selection Option
About The Copper-coated Steel (RG-45) Oxy-acetylene Gas Welding Rod, 3/32 in. x 18 in., 8 pk
Mild steel copper-coated oxy-acetylene gas welding rods are made of high-quality carbon steel of uniform and tightly controlled analysis. These rods have a melting point of 2750° F and produce quality welds of up to 65,000 PSI tensile strength. Ideal general purpose rod for welding all low-carbon steels.