Bare Bronze Gas Welding Rod 3/32 in. x 18 in., 8 pk
770510
Selection Option
About The Bare Bronze Gas Welding Rod 3/32 in. x 18 in., 8 pk
Low-fuming bronze gas welding rods. Copper-tin alloy flows easily and joins cast or malleable iron, galvanized steel, bronze, copper and steel. Melts at 1630°F; joints up to 63,000 PSI. Bare rods require flux #770119.