About The 316L Stainless 3/32 in. Stick Electrode, 5 pk
For molybdenum bearing stainless steels with 1.5 - 3.0% Mo. Primarily used for resistance to pitting, acids, and general corrosion. Maintenance quality smooth running electrode for welding most stainless steels. All position. Extra low carbon content to resist pitting. 80,000 PSI tensile strength.