7018 3/32 in. Stick Electrode, 10 lb.
770476
Selection Option
About The 7018 3/32 in. Stick Electrode, 10 lb.
Low-hydrogen electrode for all positions on low, medium and high-carbon steels. 70,000 PSI tensile, ideal for out of position welding and tacking. Runs on AC or DCEP (reverse). Not for low-voltage AC welders. Hobart recommended with Miller.