6013 3/32 in. Stick Electrode, 1 lb.
H117132-R01
Selection Option
About The 6013 3/32 in. Stick Electrode, 1 lb.
Light to medium penetrating all-purpose stick electrode for all positions on carbon steel. 60,000 PSI tensile strength. Operates on AC, DCEP (reverse) or DCEN (straight). Ideal for general use and joints with poor fit-up.