Hobart logo Trademark Logo Updated JPG
How to Weld a Rebar Snowflake l Holiday DIY

How to Weld a Rebar Snowflake l Holiday DIY

11/03/2026

How to Weld a Rebar Snowflake

Turn rebar pieces into a welded snowflake for your holiday display. Watch Braden Cowell, welding engineer at Hobart, arrange the pieces, weld the connections with the Handler® 210i and grind the finished snowflake.

 

Tools and Materials needed:


  • Hobart® Handler® 210i MIG welder
  • Welding helmet, gloves, safety glasses and protective clothing
     
  • 3/8" rebar, cut to the following lengths:
    • 8 pieces, each 9" long
    • 16 pieces, each 4" long
    • 16 pieces, each 2" long
  • 2 steel center rings
  • MIG welding pliers and tape measure
  • Angle grinder

Holiday Snowflake Project Plan

Add a handmade touch to your holiday display with a rebar snowflake. Download the easy-to-follow project plan.