.030 Contact Tip - (Pkg of 5) | HobartWelders

.030 Contact Tip - (Pkg of 5)

770177
Pack of 5 .030 inch contact tips compatible for use with Handler 125, 125 EZ, 130, 140, 190, 210MVP, TREK 180, Auto Arc Toolmate 100, IronMan 230 & later Hobart Beta-MIG 1800 and 2510 welders.
$7.99 Manufacturer Suggested Price (USD)

Specifications

General Specifications

Title .030 Contact Tip - (Pkg of 5)
Net Width 2 in
Net Height 0.75 in
Net Length 3.75 in
Net Weight 0.088 lbs
Warranty Hobart Warranty