1/8 in. Nomacast Electrode, 14 pk
H990003-RDP
Selection Option
About The 1/8 in. Nomacast Electrode, 14 pk
For various grades of cast iron, this electrode provides an excellent, non-machinable base pass for subsequent nickel alloy repairs on contaminated cast iron. AC/DC (electrode positive preferred).