7018 1/8 in. Stick Electrode, 10 lb.
770479
Selection Option
About The 7018 1/8 in. Stick Electrode, 10 lb.
Low-hydrogen electrode for all positions on low, medium, high-carbon steels. 70,000 PSI tensile strength. Ideal for out-of-position welding and tacking. Runs on AC or DCEP. Not for low-voltage AC. Compatible with Miller.