6013 5/32 in. Stick Electrode, 5 lb.
770472
Selection Option
About The 6013 5/32 in. Stick Electrode, 5 lb.
Light/medium penetrating, all-purpose stick electrode for all positions on carbon steel. 60,000 PSI tensile. Runs AC, DCEP or DCEN. Ideal for general use and joints with poor fit-up. Hobart, recommended for Miller.