6010 1/8 in. Stick Electrode, 5 lb.
770833
Selection Option
About The 6010 1/8 in. Stick Electrode, 5 lb.
Premium cellulose stick electrode for pipe and construction welding. Low spatter, easy slag removal, excellent operator control. Single or multiple pass, DCEP, all-position. 60,000 PSI tensile strength.