Select Products For Compare | HobartWelders

6013 Stick Electrodes:
Compare Packages

Select products to compare:

  1. 6013 3/32 in. stick electrode - 5 lb.

    A light to medium penetrating all-purpose stick electrode for use in all positions on carbon steel. 60,000 PSI tensile strength. Runs on AC or DCEP (reverse) polarity or DCEN (straight) polarity. Good for general, all-purpose applications and joints with poor fit-up.
  2. 6013 3/32 in. stick electrode - 10 lb.

    A light to medium penetrating all-purpose stick electrode for use in all positions on carbon steel. 60,000 PSI tensile strength. Runs on AC or DCEP (reverse) polarity or DCEN (straight) polarity. Good for general, all-purpose applications and joints with poor fit-up.
  3. 770468 Stick Electrodes

    6013 1/8 in. stick electrode - 25 lb.

    A light to medium penetrating all-purpose stick electrode for use in all positions on carbon steel. 60,000 PSI tensile strength. Runs on AC or DCEP (reverse) polarity or DCEN (straight) polarity. Good for general, all-purpose applications and joints with poor fit-up.
  4. 6013 1/8 in. stick electrode - 5 lb.

    A light to medium penetrating all-purpose stick electrode for use in all positions on carbon steel. 60,000 PSI tensile strength. Runs on AC or DCEP (reverse) polarity or DCEN (straight) polarity. Good for general, all-purpose applications and joints with poor fit-up.
  5. 6013 1/8 in. stick electrode - 10 lb.

    A light to medium penetrating all-purpose stick electrode for use in all positions on carbon steel. 60,000 PSI tensile strength. Runs on AC or DCEP (reverse) polarity or DCEN (straight) polarity. Good for general, all-purpose applications and joints with poor fit-up.
  6. 6013 5/32 in. stick electrode - 25 lb.

    A light to medium penetrating all-purpose stick electrode for use in all positions on carbon steel. 60,000 PSI tensile strength. Runs on AC or DCEP (reverse) polarity or DCEN (straight) polarity. Good for general, all-purpose applications and joints with poor fit-up.
  7. 6013 5/32 in. stick electrode - 5 lb.

    A light to medium penetrating all-purpose stick electrode for use in all positions on carbon steel. 60,000 PSI tensile strength. Runs on AC or DCEP (reverse) polarity or DCEN (straight) polarity. Good for general, all-purpose applications and joints with poor fit-up.
  8. 6013 5/32 in. stick electrode - 10 lb.

    A light to medium penetrating all-purpose stick electrode for use in all positions on carbon steel. 60,000 PSI tensile strength. Runs on AC or DCEP (reverse) polarity or DCEN (straight) polarity. Good for general, all-purpose applications and joints with poor fit-up.
  9. 6013 1/16 in. stick electrode - qty. 38

    A light to medium penetrating all-purpose stick electrode for use in all positions, on carbon steel. 60,000 PSI tensile strength. Runs on AC or DCEP (reverse) polarity or DCEN (straight) polarity. Good for general, all-purpose applications and joints with poor fit-up.
  10. H117125-RDP 6013 Electrodes Packaging RF

    6013 5/64 in. stick electrode - qty. 23

    A light to medium penetrating all-purpose stick electrode for use in all positions, on carbon steel. 60,000 PSI tensile strength. Runs on AC or DCEP (reverse) polarity or DCEN (straight) polarity. Good for general, all-purpose applications and joints with poor fit-up.
  11. 6013 3/32 in. stick electrode - 1 lb.

    A light to medium penetrating all-purpose stick electrode for use in all positions, on carbon steel. 60,000 PSI tensile strength. Runs on AC or DCEP (reverse) polarity or DCEN (straight) polarity. Good for general, all-purpose applications and joints with poor fit-up.
  12. H117144-R01 6013 Electrode Packaging RF

    6013 1/8 in. stick electrode - 1 lb.

    A light to medium penetrating all-purpose stick electrode for use in all positions, on carbon steel. 60,000 PSI tensile strength. Runs on AC or DCEP (reverse) polarity or DCEN (straight) polarity. Good for general, all-purpose applications and joints with poor fit-up.