  1. H480644-RDP 1/8 Stainless 213 Plus Electrode Packaging RF

    312 plus stainless 1/8 in. stick electrode - qty. 5

    For hard-to-weld or dissimilar metals, stainless, high-carbon, cast, and high-nickel steels. All position, AC/DC (electrode positive), easy strike and re-strike, high moisture resistance, self-detaching slag.
  2. 308L stainless 3/32 in. stick electrode - qty. 5

    For 308 and 304 stainless base metal. Smooth, tough welds with the strength, corrosion and crack resistance needed for welding stainless steel in all positions. Easy slag removal. AC or DC electrode positive (reverse) polarity.
  3. 312 plus stainless 3/32 in. stick electrode - qty. 5

    For hard-to-weld or dissimilar metals, stainless, high-carbon, cast, and high-nickel steels. All position, AC/DC (electrode positive), easy strike and re-strike, high moisture resistance, self-detaching slag.
  4. 316L Stainless 3/32 in. stick electrode - qty. 5

    For molybdenum bearing stainless steels with 1.5 - 3.0% Mo. Primarily used for resistance to pitting, acids, and general corrosion. Maintenance quality smooth running electrode for welding most stainless steels. All position. Extra low carbon content to resist pitting. 80,000 PSI tensile strength.