Nickel 55 3/32 in. stick electrode - qty. 10

Nickel 99 3/32 in. stick electrode - qty. 10

Stock # H500631-RDP H500531-RDP
Manufacturer Suggested Price (USD) See Product for Details See Product for Details
Description For repair in all positions of materials with 55% nickel cast iron. This electrode produces welds with higher strengths and ductility than the straight nickel electrodes. Deposits are machinable, but harder and more resistant to cracks and abrasion than high-nickel welds. AC/DC (electrode positive). Preheating is mandatory on cast iron. This high nickel content electrode is good for castings of light to medium weight. Welds are easily produced in all positions and the deposits are readily machined. AC/DC (electrode positive). Preheating is mandatory. Cool slowly in still air.
Title Nickel 55 3/32 in. stick electrode - qty. 10 Nickel 99 3/32 in. stick electrode - qty. 10