Compare Products | HobartWelders
  H381806-R18 H381808-R18 H383806-R18 H383808-R18
 

ER4043 aluminum wire .030 - 1 lb. spool

ER4043 aluminum wire .035 - 1 lb. spool

ER5356 aluminum wire .030 - 1 lb. spool

ER5356 aluminum wire .035 - 1 lb. spool

Stock # H381806-R18 H381808-R18 H383806-R18 H383808-R18
Manufacturer Suggested Price (USD) See Product for Details See Product for Details See Product for Details See Product for Details
Description ER4043 is a general-purpose type aluminum welding wire. It contains silicon additives, which result in improved fluidity (wetting action) of the weld pool and also produces a weld less sensitive to cracking. Its bright weld finish makes it a popular choice of welders. It can be used to weld various grades of aluminum. ER4043 is a general-purpose type aluminum welding wire. It contains silicon additives, which result in improved fluidity (wetting action) of the weld pool and also produces a weld less sensitive to cracking. Its bright weld finish makes it a popular choice of welders. It can be used to weld various grades of aluminum. ER5356 is a general-purpose type aluminum alloy, which is typically chosen for its relatively high shear strength. Offers excellent corrosion resistance when exposed to salt water. ER5356 should be used for welding 5000 series aluminum base metals. ER5356 is a general-purpose type aluminum alloy, which is typically chosen for its relatively high shear strength. Offers excellent corrosion resistance when exposed to salt water. ER5356 should be used for welding 5000 series aluminum base metals.
Title ER4043 aluminum wire .030 - 1 lb. spool ER4043 aluminum wire .035 - 1 lb. spool ER5356 aluminum wire .030 - 1 lb. spool ER5356 aluminum wire .035 - 1 lb. spool