Description |
For hard-to-weld or dissimilar metals, stainless, high-carbon, cast, and high-nickel steels. All position, AC/DC (electrode positive), easy strike and re-strike, high moisture resistance, self-detaching slag. |
For 308 and 304 stainless base metal. Smooth, tough welds with the strength, corrosion and crack resistance needed for welding stainless steel in all positions. Easy slag removal. AC or DC electrode positive (reverse) polarity. |
For hard-to-weld or dissimilar metals, stainless, high-carbon, cast, and high-nickel steels. All position, AC/DC (electrode positive), easy strike and re-strike, high moisture resistance, self-detaching slag. |
For molybdenum bearing stainless steels with 1.5 - 3.0% Mo. Primarily used for resistance to pitting, acids, and general corrosion. Maintenance quality smooth running electrode for welding most stainless steels. All position. Extra low carbon content to resist pitting. 80,000 PSI tensile strength. |