Flux coated bronze gas welding rod 3/32 in. x 18 in. - qty. 8
770512
tig-brazing-rod
Low-fuming bronze gas welding rods are made of copper/tin alloy to produce a rod that flows easily, joins a variety of metals including cast and malleable iron, galvanized steel, bronze, copper and steel. These rods have a melting point of 1630° F and produce strong joints up to 63,000 PSI tensile strength.