MIG Aluminum wire, ER5356 .030" 1 pound | HobartWelders

ER5356 aluminum wire .030 - 1 lb. spool

H383806-R18
ER5356 is a general-purpose type aluminum alloy, which is typically chosen for its relatively high shear strength. Offers excellent corrosion resistance when exposed to salt water. ER5356 should be used for welding 5000 series aluminum base metals.

Specifications

General Specifications

Title ER5356 aluminum wire .030 - 1 lb. spool