No. 4 Gauge Flex Welding Cable - 250 Ft. Spool

770113F
#4 AWG 99.9% copper welding cable. Consists of one bare copper conductor with rubber insulation jacket. Cut and sold by foot to desired length.

Features

Standards
RoHS Compliant, ASTM B3, B172
Resistivity
Max at 68 F (20 C), Max conductivity of 100 IACS
Temperature
-58 F to 221 F (-50 C to 105 C) EPDM insulation for optimum cold weather
Conductivity Wire Size
4 AWG welding cable resists oil, chemicals, water, ozone and solvents
Conductor
ETP Copper 99.9% (UNS C 11000), Rope-lay, Stranded
Rating
600 volts applications

Specifications

General Specifications

Title No. 4 Gauge Flex Welding Cable - 250 Ft. Spool