Since my LWS is closed this holiday weekend and I can't make it up there this week during work, I am looking for a tip for brazing thin (20ga-22ga) sheet metal. From the Victor site, it recommended a 000 welding nozzle.
I'm finding two types; one that is for a 'clamshell' and the other doesn't specify. Does this make sense?
weldingsupply have mpn# 034-0068:
http://weldingsupply.securesites.com...4-0068||1|751|
ram welding shows it as mpn# 0387-0028:
http://www.ramweldingsupply.com/prod...ew.mcic?s=1178
Both W-1 series. My torch is a WH26FC, so I think either will work, but not sure the difference...any idea?
ram welding supply is pretty close to me, so shipping would be faster. I know it'd be best to take my torch to the LWS, but if I could mailorder, I'd have it for next weekend.