Old 07-12-2010, 03:57 PM
OneWelder OneWelder is offline
Junior Member
 
Join Date: Feb 2009
Posts: 22
I can tell you my experience - I have used both Acetylene and propane since the the sixty's - I have never had a problem swapping Acetylene to propane reg
As far as the hoses go well on one of the trks three of the four hoses have been on there since 1990 . Hoses are not cracked , are still pliable in fact show no signs of there age ( propane on the trks - Acetylene in the shop)
- hoses are the R
Thats just my experience you should do what you think is right
Reply With Quote
 


Thread Tools
Display Modes Rate This Thread
Rate This Thread:




Please read our Terms of Use. Messages that harass, abuse or threaten other members; have obscene or otherwise objectionable content; have spam, commercial or advertising content or links may be removed and may result in the loss of your posting privileges. Please do not post any private information unless you want it to be available publicly.

Powered by vBulletin® Version 3.8.3
Copyright ©2000 - 2010, Jelsoft Enterprises Ltd.