    Silver solder

    Anyone know of a good online source to get silver solder in the bigger rolls?
    The Maniacal Migging Guy {as Hankj would put it}


    HH180
    Cutmaster 51

  2. #2
    Join Date
    Sep 2002
    Location
    Central Kali
    Posts
    5,292
    How big a roll do you want? A little goes a long way.

  3. #3
    Join Date
    Jun 2004
    Location
    Sadorus Il
    Posts
    976
    Not sure of the weight but the rolls are about 5 in in diameter.and about 2 inches thick. I found what i was looking for on the harris site but there are no prices listed,
    The Maniacal Migging Guy {as Hankj would put it}


    HH180
    Cutmaster 51

  4. #4
    Join Date
    Sep 2002
    Location
    Central Kali
    Posts
    5,292
    Does $10 per pound sound about right? Of course it depends on the silver content. Or is that $10 per oz?

  5. #5
    Join Date
    Mar 2004
    Location
    maple ridge, BC
    Posts
    92
    forget the rolls buy it in rod form with the flux already on it...way better. its $$$$$ but high silver content is what u want anyway.
    AmaC
    MM175
    O/A torches
    snap on everything

  6. #6
    Join Date
    Nov 2004
    Location
    NJ
    Posts
    16
    are you looking for solder with silver content or brazing rod ? 2 totally different animals

  7. #7
    Join Date
    Jun 2004
    Location
    Sadorus Il
    Posts
    976
    solder that comes in rolls. used primarily to repair aluminum radiators in the newer cars.
    rods would be fine but wont fit on the rig i have set up to put rolls on and pull out and use what i need and just let it hang.The desination is AWS A5.8 B Ag 5 (i think the last number is 5)theres a # 45 on the roll also.
    The Maniacal Migging Guy {as Hankj would put it}


    HH180
    Cutmaster 51

  8. #8
    Join Date
    Nov 2004
    Location
    NJ
    Posts
    16
    to solder aluminum you should use "alsolder 500" w/ stay clean aluminum flux and to braze it you should use "al-braze 1070" w/ albraze aluminum powder flux if your going with jw harris. They are the best for alum to alum joints.

  9. #9
    Join Date
    Jun 2004
    Location
    Sadorus Il
    Posts
    976
    The stuff i have now works great,just trying to find it cheaper.
    The Maniacal Migging Guy {as Hankj would put it}


    HH180
    Cutmaster 51

  10. #10
    Join Date
    Jan 2004
    Location
    Browns Valley, CA
    Posts
    8,518
    MM (alis "70")

    Response on other board...

    Hank
    ...from the Gadget Garage
    MM 210 w/3035, BWE
    HH 210 w/DP 3035
    TA185TSW
    Victor O/A "J" series, SuperRange
    Avatar courtesy of Bob Sigmon...

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •