Anyone, I have a set procedure to follow on this job I am working on. Using ER90SB3 for the TIG root and E9018B3 Stick to fill. I was wondering how others would do this job. What temperature do you preheat to and do you prefer gas backing for the root run ? I have several butt welds to make and I have mostly welded P11 in the past so this P22 Material I am told has to be done in a careful manner. The job will be heat treated when finished along with xray. Any thoughts or comments would be greatly appreciated. FrankCC