    i'm going to use gas to start with,which gas would be best c25 or 75 argon 25co2? i am open for sugestions or comments. looking at an 80cu.ft. tank. chumly.

  2. #2
    Join Date
    Sep 2002
    Location
    Jefferson, Maryland
    Posts
    345
    C25 is 25% CO and 75% argon.

    Its what I use and the Miller GMAW book also recomends it.
    It's not an optical illusion...it just looks like one

  3. #3
    Join Date
    Jan 2003
    Location
    central city,iowa
    Posts
    31
    i feel like that was a dumb question,i'll ask one more, at thiesens i noticed they handle k-t industries wire. is this good wire? who is it made by? chumly.

  4. #4
    Join Date
    Sep 2002
    Location
    Jefferson, Maryland
    Posts
    345
    Any question finds a home here, keep asking and don't stop.

    Not sure about the k-t industries brand, I'm new at this too!

    I've heard, stick with the brand names or it won't stick. sorry
    It's not an optical illusion...it just looks like one

  5. #5
    Join Date
    Jan 2003
    Location
    knoxville
    Posts
    5
    You could use 98% argon 2% o2 and spray for good wetting it burns in real good (not for sheet metal)
    Br1@n

  6. #6
    Hobart Expert Rock Guest

    Thumbs up

    CHUMBLY..........NO DUMB QUESTIONS HERE, THE ONLY DUMB ONES ARE THE ONES THAT DON'T GET ASKED..........IF MONEY IS THE ISSUE ON GAS TYPICALLY THE MORE BLENDS THE MORE EXPENSIVE, AS I RECALL THE LEAST EXPENSIVE GAS OUT THERE IS CO2....................HOWEVER CO2 TENDS TO BURN A LITTLE HOTTER THAN SAY ARGON/CO2..........................KEEP THE QUESTIONS COMMING THERE ARE A MULTITUDE OF EXPERIENCED FOLKS ON HERE TO HELP OUT.......................ROCK
    SSCOTT@MILLERWELDS.COM

  7. #7
    Join Date
    Dec 2002
    Location
    Bend, Oregon
    Posts
    23
    hey Hobart expert rock, just wondering... why is your font always on caps?
    on some other forums i go to, having your caps on means your yelling.

  8. #8
    Hobart Expert Rock Guest
    SUPER VW.........I KNOW BUT JUST ABOUT EVERYONE EXCEPTS IT NOW AS JUST THE WAY IT IS..........THEY ARE LOCKED BECAUSE IN SERVICE FILLING OUT WARRANTY CLAIMS ALL WORDS ARE IN CAPS..........AND SINCE I'VE DONE BUNCH'S, AND I AM AN OLD GUY (OFFICIAL JUST ASK MY KIDS), IT IS VERY HARD TO BREAK A HABIT YOU'VE BEEN DOING FOR 20 SOME YEARS..............BELIEVE ME I NEVER HOLLER,YELL, ETC.......... MIGHT CURSE BUT THAT IS ABOUT IT..................GOOD QUESTION..............HONEST ANSWER.......ROCK
    SSCOTT@MILLERWELDS.COM

  9. #9
    Join Date
    Sep 2002
    Location
    San Diego, CA
    Posts
    7,704
    Originally posted by super vw
    hey Hobart expert rock, just wondering... why is your font always on caps?
    on some other forums i go to, having your caps on means your yelling.
    We all got on him for doing that, but we now accept it that when ROCK types in all caps...it's not yelling, just good common sense help for all us weldors. He is the exception to the rule. And that's OK.
    Arcin' and sparkin', Rocky D <><
    Experience is something you don't get until just after you need it.
    IF YOU CAN READ THIS, THANK A TEACHER...
    IF YOU'RE READING THIS IN ENGLISH, THANK A SOLDIER!

  10. #10
    Join Date
    Dec 2002
    Location
    Bend, Oregon
    Posts
    23
    Alrighty then... i was just wondering, not sayin that you yell alot .