    Question miller snapstart

    Hi guys, need help, can a snapstart HF unit for the older maxstars be adapted to a miller dialarc 250 and used to tig alum.?

    grin1

  2. #2
    Join Date
    Dec 2002
    Location
    fremont, wi
    Posts
    27

    snapstart

    The Miller Snapstart will not work for tig alum. welding on the Dialarc 250. The HF is only on for the start and not continuous.
    Thank you

  3. #3
    Join Date
    Dec 2002
    Location
    toledo
    Posts
    9

    Cool

    thank you Matt. glad i did not purshase it.
    thanks, Neil