    sorry i took so long in posting the pics of the holders for you ....anyway, better late than never.
    Attached Images Attached Images
    how's that taste, happy crappy??!!?

  2. #2
    Join Date
    Feb 2004
    Location
    hill country Texas
    Posts
    228

    two

    closeup
    Attached Images Attached Images
    how's that taste, happy crappy??!!?

  3. #3
    Join Date
    Sep 2002
    Location
    South Central Kansas
    Posts
    518
    trashcan, thanks for the pictures, they are pretty cleaver looking. I might see if I can make up a few of them this weekend. Thanks Again Gerald

  4. #4
    Join Date
    Jan 2004
    Location
    PRK, USA
    Posts
    699
    trashcan,
    Noticed you made right and left handed ones so the vertical leg points up on all of them. Nice detail I would have overlooked.

  5. #5
    Join Date
    Feb 2004
    Location
    Louisiana
    Posts
    57
    Looks pretty good.

    I work all day on a 5'X10' table and I always have (3) 4.5" grinders in front of me. 1 with cutoff wheel 1 with flap disc and 1 with grinding wheel.

    My current "holder" was fashioned from some 4" flat bar with angle iron welded onto it to create "funnel" type holders. I welded the flat bar to the front of the table. Recently I have decided to make another "holder" with some "man size" magnets so that I can move the arrangement around the table with me as I go.

    Anyway....my 2 cents.