    the gun arcs even if the trigger is not depressed its not a gun problem

  2. #2
    Join Date
    Sep 2002
    Location
    San Diego, CA
    Posts
    7,704
    I would first look at the trigger wiring ...a short somewhere along the wire would do that. I do remember that there was a similar problem with a HH135 I had, wire would be hot when you turned the machine on, and no wire was feeding. Problem in the board.