    I have had 1 very good repair project with this rod.I would like to buy more but the price at 65/85$ a pound is a bit beyond my means.Any body out there want to share a 10LB can?This is a no pre or post heat and no peaning process.The weld IS machinable.This stuff is the answer to cast iron fixes.phone me to chat it up 360-966-7700 Mark
    Last edited by markodavid; 06-28-2012 at 12:36 PM. Reason: add pert. facks

  2. #2
    Join Date
    Dec 2010
    Posts
    89

    Well?

    How much do you need to do your project?
    I maybe willing to sell a pound or two