    norseman drill bits

    i think i only have two left hand bits and thought i could use some more. i was thinking about this brand. anyone use them?

  2. #2
    Join Date
    Mar 2010
    Location
    SE Michigan
    Posts
    2,071
    Mike....

    Get yourself some Cleveland Twist LH 180 split point's and don't look back.
    So little time...So many machine tools.........
    www.flipmeisters.com

    Miller, Hobart & Lincoln TIG/MIG/-
    Hypertherm Plasma (Thanks Jim)
    Plasma-Cam DHC (coming shortly)
    Harris OA
    Too many motorcycles.............-

  3. #3
    Join Date
    Apr 2009
    Location
    houston pa
    Posts
    1,286
    i cant find them online. the prices of the sets i have found by them are maybe more than im willing to pay new. maybe a broken set will show up on ebay.

  4. #4
    Join Date
    Jan 2003
    Location
    GA
    Posts
    187
    The Norseman have always been good for me.

    I've got some that are about 10 years old and they still make good holes.
    Mine are all right hand, but I can't see that making a difference.

  5. #5
    Join Date
    Nov 2005
    Location
    S.E. Wisconsin
    Posts
    4,472
    Quote Originally Posted by BMB View Post
    The Norseman have always been good for me.

    I've got some that are about 10 years old and they still make good holes.
    Mine are all right hand, but I can't see that making a difference.
    They say the lefthanded ones are smarter, but ......... I don't know?