Where can I get consumables for this unit it seems like they have all the sudden gone out of busisness. I checked them out before i bought the machine but now they are no where to be found.![]()
Where to Buy
Service & Support
e-Learning
Weld Talk
Where can I get consumables for this unit it seems like they have all the sudden gone out of busisness. I checked them out before i bought the machine but now they are no where to be found.![]()
Consumables will be applicable to whatever torch it has. Most manufacturers utilize supplied torches so you need to ascertain the make of torch and get the appropriate consumables.
So little time...So many machine tools.........
www.flipmeisters.com
Miller, Hobart & Lincoln TIG/MIG/-
Hypertherm Plasma (Thanks Jim)
Plasma-Cam DHC (coming shortly)
Harris OA
Too many motorcycles.............-
I believe the importer for Riland passed away last year. Jump over to Welding Web and ask around on the Everlast and Longevity sections of that forum for assistance. You should be able to come up with consumables for your ChiCom plasma. My plasma wasn't quite the bargain, but I only need to drive downtown for parts and service...
http://weldingweb.com/index.php
Miller 251, Lincoln PrecisionTig 275, Miller DialArc 250 AC/DC, Hypertherm 900, Bridgeport J-head, Jet 14" lathe, South Bend 9" lathe, Hossfeld bender with a collection of dies driving me to the poorhouse, Logan shaper, Ellis 3000 bandsaw, Royersford drill press and a Victor Journeyman O/A.
You can't drive to China?![]()
So little time...So many machine tools.........
www.flipmeisters.com
Miller, Hobart & Lincoln TIG/MIG/-
Hypertherm Plasma (Thanks Jim)
Plasma-Cam DHC (coming shortly)
Harris OA
Too many motorcycles.............-
Hey sclaus,
I had a Riland Cut60J that died last year & finally got a resolution while they were still in business(replacement that I sold & bought a TD Cutmaster52). I had the xtra consumables in a bag hanging in the shop that I forgot I had. Here's a pic. I want $40 & that includes shipping. PM me if interested.
Denny
Complete weld/mach./fab shop
Mobile unit
"A man's word is his honor...without honor, there is nothing."
"Words are like bullets.... once they leave your muzzle, you cannot get them back."
"I have no hesitation to kill nor reservation to die for the American Flag & the US Constitution."