    Stainless steel handrail warping

    I am going to be fabricating a interior stainless steel hand rail. It will likey have a round 1 1/2" D. 1/8" wall hand rail, with round 1" D. 1/8" wall pickets apx 4-5" on center spacing. This rail will be on a stair case, so the pickets will be coped to rail on about 32 degrees. GTAW is the process. My concern is that the top rail is going to have waves in it from all the welding of pickets. My Question, is there any tricks to prevent the top rail from warping. How to keep the top rail totally staight. The longest rail stetch is apx 10'- 12' long. I was thinking fusing without filler might help. If you have any tricks or tips that can help keep my rail staight and prevent warping. I would greatly appreciate any helpful insight.

  2. #2
    Join Date
    Sep 2002
    Location
    PCB, Fl
    Posts
    3,940
    Easy sure way to have no warping is do not weld it. Drill holes and insert pickets.
    Roger

  3. #3
    Join Date
    Mar 2011
    Posts
    155
    Quote Originally Posted by Roger View Post
    Easy sure way to have no warping is do not weld it. Drill holes and insert pickets.
    That is what I would do. You have to know when to not weld.

  4. #4
    Join Date
    Jul 2005
    Location
    Missouri
    Posts
    51

    Wink

    Originally Posted by bvweld
    Just FYI, I saw your post from some time ago,but might help some others. This will help your distortion issue along with controlling your heat and moving around. Check this link:

    http://www.stagesmith.com/gallery/sh...amp/index.html
    Done a few rails some in stainless.Pictures are self explanatory, you will get the idea

  5. #5
    Join Date
    Aug 2011
    Location
    Canada
    Posts
    5
    the clamp is a good idea, another tips wich is also good for any type of pickets on any type of railing is weld 1 and pass 1 between each one, if the railing is really long like 8, 9, 10 stairs and more you can pass 2 pickets at the time, you do the bottom and the top the same way, i know its look longer but the job i better!

    for the big clamp i prefer to use it on central tube of railling and stuff like that!

  6. #6
    Join Date
    Jun 2012
    Posts
    1

    Stainless steel handrail warping

    I think that steel is very important and useful metal.You can use clamp and three holding angle which is very useful for your stainless steel hand rail.I think u must have used welding of pickets. You must remember that heat is keeping minimum around the rail.

  7. #7
    Join Date
    May 2013
    Posts
    1
    Instate stainless steel on your railing and you will have the best cable railing for your deck or balcony.

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •