    i am doing a job test next week and i am having trouble with it it is overhead beveled carbon steel 1/8th root what i am to do is do the root with 7018 and weld it all out then gouge out the back what the problems is there a trick to getting the rod to flow nice to fill th root nice and smooth etc your tips and advice would be greatly appreciated

  2. #2
    Join Date
    Sep 2002
    Location
    San Diego, CA
    Posts
    7,704
    The only trick I know is the right heat, and plenty of practice.
    Arcin' and sparkin', Rocky D <><
    Experience is something you don't get until just after you need it.
    IF YOU CAN READ THIS, THANK A TEACHER...
    IF YOU'RE READING THIS IN ENGLISH, THANK A SOLDIER!

  3. #3
    Join Date
    Mar 2003
    Location
    Brethren, Mi
    Posts
    11,282
    I would say the trick is to get the face of the root in nice and smooth and not worry so much about the back since its going to be gouged out anyway, whats this test for?

  4. #4
    Join Date
    Jan 2008
    Posts
    13
    boiilermaker job building tanks!

  5. #5
    Join Date
    Apr 2009
    Location
    Oklahoma transplanted from michigan
    Posts
    26
    not to be a di@# but maybe you need much more experience..... with those welds being smooth and nice,,,,,, aren't getting good fusion and penetration are not achieved so you need lot's more practice...to not have inclusions and pass x-ray tank or pipe tests,,, or get someone to sneak it for ya and promise not to weld pressure vessels ,maybe do some fitting....till you get it down enough to do a safe job GOOD LUCK!!!
    Lincoln 225 Tombstone,
    Hobart 180,150' Argon,
    A/D Hobart hood
    22 Ton Husky Log splitter,
    79 F350 dump eats 4.75 TONS and still turns
    20 GAL. parts washer,
    cutters,grinders,
    And a Hypertherm POWERMAX 30,has joined the family