I got a call yesterday from one of my mom pop machine shop accounts.....This is what they had for me to weld up
![]()
Where to Buy
Service & Support
e-Learning
Weld Talk
I got a call yesterday from one of my mom pop machine shop accounts.....This is what they had for me to weld up
![]()
They cut a weld prep in the flange
too wide so I had to run a bead around the hole and fill it up a bit..
The customer was afraid that there would be too much heat on the joint....
I did what they said even though I don't think there would have been a problem (I purged the tube) Oh and yes I have people hanging out at my shop all the time....This guy is one of my
bigger friends...6' 5" 310 lbs sheet rocker....