This is the first time I welded 304 SS metal. I am using a MM 250X with .035 304 SS wire. I am using TriMix gas. I get a lot of Brown overspray on both sides of the weld. The welds are holding good after I grind them down flush with the existing metal. I tried different heat settings but there is no change. Is this normal? I attached a few pictures.
Thanks, Jim