Hey 22Car,
Hobart has a Owners Manual Section that has CyberTig machines listed which will tell you how to move or install jumpers to convert to 230.
Try this link,
http://www.hobartwelders.com/owners_manuals/
Hope it helps
22CAR........ IF BUFFALO WELDING SUPPLY DOESN'T HAVE A BOOK ON IT THEN YOU WILL HALFT TO CHECK WITH SOME OLDER DISTRIBUTOR, SERVICE SHOPS WHO PROABABLY HAVE ONE THEY CAN PRINT OFF FOR YOU.........ROCK
SSCOTT@MILLERWELDS.COM
Hello 22 car. Any luck on your wiring job? If you have not found any info yet I can pop the cover on one of mine and and get you going. I wire up so much stuff in a week I can't remember all of it (might be getting old). Awesome welders, built like a tank. I have two in service, Great ***** O Fire and Joltin Jenny. (nose art) Anyway, good luck.
YES I GOT A OWNERS MANUAL FROM HOBART AND REWIRED IT.