    My plan is to build a 5x14 foot trailer designed mainly for hauling two atvs and the occasional load of lumber. The trailer will have a single 3500 lb axle.

    Would 4x5.4 channel work for the frame if I used 3x4.1channel for a wrap-around tongue? Crossmembers would be 3" channel on 24" centers.

    If 14 feet is too long for the frame, I can shorten the length down to 12.5 feet, but would prefer to have the 14 feet so I can position the load properly.

  2. #2
    Join Date
    Jun 2006
    Location
    Wichita, KS, USA
    Posts
    4,102
    I have a 12' trailer with 3" channel (don't remember the weight, but it's the lightest weight) for the frame and a 4" channel wrap-around tongue. I had to add a piece of 1.5" angle to the bottom to keep it from flexing too much, but it seems to do okay now. I use it to haul cars up to about 3k#. If the bed came as far forward as most trailers, it would be a 14' trailer, but I left the bed back just far enough that a car with its tires against the front rail is about 3.5 feet from the tailgate.

    Based on my experience, a 4" channel would probably be fine. Consider that it's not uncommon for a 7k# trailer use 5" channel.

    Just my 2.4 cents.

    Dave
    Still building my new old truck - see the progress!
    http://www.ford-trucks.com/forums/65...-coe-idea.html
    http://www.hobartwelders.com/weldtal...ad.php?t=27017

    Red (not lincoln) inverter TIG/Stick
    MM180
    SP125+

  3. #3
    Join Date
    May 2007
    Posts
    11
    Thanks for confirming what I suspected.

  4. #4
    Join Date
    Dec 2006
    Location
    southeast tx.
    Posts
    180
    threadkiller you could contact dabar39 he builds alot of trailers he freqents the miller sight more than here, anyway are you going to make the trailer a side loader for you atv's?