hey all. i've been playing with my ta 185 tsw. please let me know what you think of the weld i did this morning. i welded a 3/8 grab hook to a piece of 3/8 plate MS. the edge of the hook was beveled at roughly 45 degees. tig weld, 1/8 electrode, 185 amps, 100 % argon gas, no filler rod. i realize there is undercut on the hook itself. i am more interested in the appearance and quality of the bead itself. i am still in some need of practice adding filler rod. it seems to boil and bubble with porosity as the end result. so anyway, am i on the right track here? any and all suggestions are much appreciated.
Where to Buy
Service & Support
e-Learning
Weld Talk


Reply With Quote
You need the filler and you won't get the bubbling. I wouldn't have done that type of joint with TIG either...too much heat input....destroys the integrity of the hook...first choice would be stick, then MIG.