    Flux won't melt

    I just bought a new box of 6013 electrodes, and I can't get the flux to melt. I have to grind the electrode into the work, or or the rod melts so far up inside that it breaks the arc. I just finished the old box of rods on the same project with no problems. Same setup, same temp. What's up?

  2. #2
    Join Date
    Nov 2005
    Location
    S.E. Wisconsin
    Posts
    4,541
    I used to make the packing guides where the fluxxing agents were forced into possition for baking ........the customer described how it works ......
    Fascinating !!
    Sounds like the mix is a-fowl ....overly vitrified !!?

    I beleive you have a Bad Batch there .....take a few rods with the metal melted out , and get them relaced ..../....refunded!

    Phil


    In the beginning, the Earth was without form, and void.
    When one picks up some wood or metal or stone and shapes it into something usefull
    ... I beleive that it has to be a deliberate effort to disavow a creator.

    As you work these, and join them, you feel the force and the will of He
    who formed and shaped the very resorces that you now add your will and force to.
    Further one surely can know when your will and force is not aligned with His.

  3. #3
    Join Date
    Mar 2007
    Location
    Iowa
    Posts
    2
    Never had this problem before, so didn't have a clue. I spent the last three hours surfing the internet (found nothing), and got help here in 5 minutes! Thanks!

  4. #4
    Join Date
    Jan 2004
    Location
    Browns Valley, CA
    Posts
    8,518
    Yep, bad batch! Your LWS should swap 'em with no squawk.

    Hank
    ...from the Gadget Garage
    MM 210 w/3035, BWE
    HH 210 w/DP 3035
    TA185TSW
    Victor O/A "J" series, SuperRange
    Avatar courtesy of Bob Sigmon...

  5. #5
    Join Date
    Mar 2006
    Location
    springvale maine
    Posts
    206
    What they said
    garthswelding@aol.com one welding truck trailblazer 301g w/ spool/mig/plasma/drill press/ band saw/ and all the other stuff to do this/and air compresser

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •