Well, after going through the motions up at the shop this past weekend with my Synchro180 using er70s 2 and 6, I came to the conclusion that I am either cursed or that all the filler I bought from weldingsupply.com was badI cleaned it with acetone and proceded to weld some mild steel. Sparklers everywhere. Little volcanos constantly. Whipped out some 309stainless rod and poof, no problems at all. Nice, smooth beads. I didn't have any problems with the SS filler rod. I'm kinda pissed about the whole deal actually. I have about 20lbs of mild steel filler rod that's gonna get wasted. Any other suggestions before it gets recycled
![]()
Where to Buy
Service & Support
e-Learning
Weld Talk


I cleaned it with acetone and proceded to weld some mild steel. Sparklers everywhere. Little volcanos constantly. Whipped out some 309stainless rod and poof, no problems at all. Nice, smooth beads. I didn't have any problems with the SS filler rod. I'm kinda pissed about the whole deal actually. I have about 20lbs of mild steel filler rod that's gonna get wasted. Any other suggestions before it gets recycled
Reply With Quote