octopod
01-23-2003, 09:18 AM
does anybody have any infor mation on E7411 rods?
uses? manufacturers? etc.
just found some laying around here at school and no one seems to know anything about them.:confused:
Mike Sherman
01-23-2003, 10:06 AM
I would like to see that electrode. It is not a current AWS designation that I am aware of. Is it smudged and barely legible? If possible can you post a picture of it??
octopod
01-23-2003, 12:30 PM
i don't have any more of them there were only two half burned rods. And i used them in order to see how they burned. I can tell you that they said 7411 on them, and the coating was green and that the beads were like butter.
Nicest beads i have everseen.
out of any process