could someone explain to me the pro's & con's of DC +&- . have welded enough to get me buy but am triing to learn to do it proper.thanks

Hobart Expert Rock
01-16-2003, 08:05 AM
HI BARTH..........LET'S TALK ABOUT WELDING RODS SHALL WE. WHEN YOU BUY THE ROD OF YOUR CHOICE IF YOU NOTICE ON THE LABEL SOME RODS SAY DCEP (DC+) AND SOME SAY DCEN (DC-) AND SOME SAY DCEP/DCEN...........THEY'RE TELLING YOU THE POLARITY THE ROD WILL RUN IN FOR OPTIMUM PERFORMANCE. THIS WILL ALSO EQUATE TO WELDING WIRE'S ETC...........OPTIMUM........ BEING THE KEY HERE FOR PENETRATION AND STRENGTH........................IF YOU NEED A QUOTE FROM A WELDING MANUAL I CAN PROVIDE I JUST THOUGHT MAYBE THIS WOULD EXPLAIN IT..............................ROCK
SSCOTT@MILLERWELDS.COM

Roger
01-16-2003, 08:24 AM
Download one of these owners manuals for type of welder you have. They have some great information and drawings on how POLARITY affects welds.
http://hobartwelders.com/owners_manuals/