skinner
01-05-2003, 09:28 PM
can anyone tell me who made the napa handyman mig welders and maybe where to get parts for them such as liners , rollers and such.
brianw
01-06-2003, 09:34 AM
century makes alot of the private labeled machines, they are now part of clore automotive, 1-800-328-2921. May want to check with napa first if you have not done so. Make sure to have model and serial number ready if possible. Good luck